Features
1) Low temperature resistance ( 88-120 °C)
2) Excellent resistant to hydrolysis, acids and alkalies
3) Smooth surface, more defined pore size and good air permeability
4) Lower fiber release, Lower density,High mechanical characteristics
Physical and Chemical properties
| Weight(gs/m) | 500 | |
| Thickness(mm) | 2 | |
| Width(mm) | ≤2.2 m | |
| Finish treatment | Singeing, Calendaring, Heat setting | |
| Air permeability(L/m2.s) | 150-200 | |
| Tensile strength(N/5 cm) | warp | ≥1700 |
| weft | ≥2200 | |
| Tensile elongation(%) | warp | ≤20 |
| weft | ≤30 | |
| Heat shrinkage(%) | warp | ≤1.5 |
| weft | ≤1.0 | |
| Temperature(°C/°F) | Continue | 90 /194 |
| Instant | 120 /248 | |
| Anti-acid | Excellent | |
| Anti-alkali | Excellent | |
| Anti-abrasion | Good | |
| hydrolysis stability | Excellent | |
Specifications
| Para | Weight (g/sm) | Thickness (mm ) | Air Permeability (m3/m2/min) | Tensile Strength (N/5×20cm) | Tensile Elongation(%) | Operating Temp.
(°C/℉) |
Max Surge Temp.
(°C/℉) |
Suitable P.H. value | ||
| Model | / | / | / | Warp | Weft | Warp | Weft | / | / | / |
| PP-01 | 550 | 3.5 | 10 | 1000 | 1500 | 50 | 50 | 130/266(Dry Heat) | 150/302 (Dry Heat) | 1~12 |
| PP-05 | 400 | 2.5 | 20 | 500 | 1000 | 60 | 60 | 1~12 | ||
| PP-10 | 400 | 2.2 | 24 | 500 | 1000 | 80 | 80 | 1~12 | ||
| PP-25 | 400 | 3 | 35 | 500 | 1000 | 85 | 85 | 1~12 | ||
| PP-50 | 320 | 3.5 | 100 | 500 | 600 | 100 | 80 | 1~12 | ||
| PP-75 | 320 | 3.5 | 130 | 500 | 600 | 100 | 80 | 1~12 | ||
| PP-100 | 350 | 3.8 | 100 | 500 | 500 | 100 | 100 | 1~12 | ||
| PP-200 | 400 | 3.8 | 130 | 500 | 600 | 110 | 100 | 1~12 | ||